SARBAK METAL TİC. VE SAN. A.Ş.

SARBAK METAL TİC. VE SAN. A.Ş.
Sarbak Publication Date: 09.05.2014
UBA Revision Date: 20.12.2013 3. Rev.
ALLOYS LISTED IN UBA’S HYGIENIC LIST
DW509L - CuZn40
DW510L - CuZn42
DW511L - CuZn38As
DW612N - CuZn36Pb2
DW617N - CuZn40Pb2
DW603N - CuZn36Pb3
DW614N - CuZn39Pb3
DW626N - CuZn33Pb1,5AlAs
DW724R - CuZn21Si3P
CB752S - CuZn35Pb2Al-B
Please specify on order , if hygienic list compliance needed.
For CW511L and CW626N alloys after the forging process, heat
treatment should be 2 hours at 500 °C for meeting the conditions of
EN ISO 6509. According to process conditions, temperature and time
can be change.
OUALITY MANAGER
ŞİRİN BİLGİN
Dijital olarak imzalayan Sirin
Bilgin
DN: cn=Sirin Bilgin, o=Sarbak
Metal, ou=Kalite,
[email protected],
c=TR - TÜRKİYE
Tarih: 2014.05.09 16:14:05
+03'00'
FACTORY MANAGER
TUĞHAN ÖZÇAMSIRTI
Dijital olarak imzalayan Tughan
Ozcamsirti
DN: cn=Tughan Ozcamsirti,
o=Sarbak Metal, ou=Fabrika
Muduru,
email=tughanozcamsirti@sarbak
.com.tr, c=TR - TÜRKİYE
Tarih: 2014.05.09 16:13:53
+03'00'